鋁塑板染不上色你知道是為什么嗎?

來源:http://m.speif.com/ 發布時間:2019-01-17

跟著工藝技術的開展,鋁塑板在人們生活中運用的重量越來越高,在色彩方面也不再像曾經那樣單調。現在的鋁塑板加工
With the development of technology, the weight of aluminium-plastic sheet used in people's life is getting higher and higher, and its color is no longer as monotonous as it used to be. Current Aluminum Plastic Plate Processing
可以對你想要的顏色進行上色,但我們在對鋁塑板上色時,難免會遇到染不上色的狀況,那么,鋁塑板染不上色的發生原
You can colour the color you want, but when we colour the aluminium plastic sheet, we will inevitably encounter the situation that the color cannot be dyed. Then, the origin of the color cannot be dyed on the aluminium plastic sheet.
因及處理方法有:
The causes and treatment methods are as follows:
1、陽極氧化膜厚不足:解決的辦法是檢查陽極氧化工藝是否規范,看溫度,電壓,導電等要素是否穩定,若有異
1. Insufficient thickness of anodic oxide film: The solution is to check whether the anodic oxidation process is standardized and whether the factors such as temperature, voltage and conductivity are stable, if different.
常,請相應調整規范之,若無異常,可恰當延長氧化時間,確保膜厚合格。
Often, please adjust the specifications accordingly. If there is no abnormality, the oxidation time can be prolonged appropriately to ensure that the film thickness is up to standard.
2、染液PH值太高:此刻,可用冰醋酸將PH值調至規范值。
2. The PH value of dye solution is too high: at this moment, the PH value can be adjusted to the standard value by glacial acetic acid.
3、氧化后工件在水槽中放置時間太久:發起及時染色,假如這種狀況現已發生,可將工件放在陽極氧化槽中或硝
3. After oxidation, the workpiece is placed in the tank for too long: initiating timely dyeing, if this situation has occurred, the workpiece can be placed in the anodic oxidation tank or nitrate
酸中和槽中恰當活化處理后再進行染色,效果會很好。
Appropriate activation treatment in acid neutralization tank before dyeing can achieve good results.
4、選用染料已分解或霉變:此刻需更換染料,選用適宜染料。
4. Choose dyestuffs that have been decomposed or moulded. At this moment, dyestuffs need to be replaced and suitable dyestuffs should be selected.


5、氧化溫度過低,導致皮膜致密:可恰當進步氧化溫度。
5. Low oxidation temperature results in dense skin film: oxidation temperature can be properly improved.
6、導電不良:可能陽極銅桿或陰極鉛板接觸不良所示批量導電不良。留意清洗陽極銅桿及陰極鉛板,確保導電良
6. Poor conductivity: Batch conductivity shown by poor contact of anode copper rod or cathode lead plate may be poor. Pay attention to cleaning anode copper rod and cathode lead plate to ensure good conductivity
好。
OK.
以上就是關于鋁塑板染不上色的發生原因及處理方法,現在,鋁塑板現已成為建筑范疇的常用材料,其廣泛用于大樓
Above is about the causes and treatment methods of stainless aluminium-plastic sheet. Now, aluminium-plastic sheet has become a common building material, which is widely used in buildings.
外墻、室內墻面、廣告招牌等裝修用范疇。然而跟著人們對裝修用品的美觀要求越來越高,色彩單一、圖畫呆板的鋁塑板
Exterior walls, interior walls, advertising signs and other decoration areas. However, along with people's increasingly high aesthetic requirements for decoration supplies, single color, stiff drawing of aluminum-plastic sheet
現已無法滿意出產需求。
It is no longer able to satisfy the production demand.
以上信息是我們鋁板生產廠家整理發布希望對大家有點幫助我們的網站是:http://m.speif.com
The above information is our aluminium plate manufacturer collation and release hope to help you a little bit: http://m.speif.com!

主站蜘蛛池模板: 巨爆中文字幕巨爆区爆乳| 精品人妻系列无码一区二区三区| 国产精品熟女视频一区二区| 国产亚洲无线码一区二区| a级毛片免费观看在线| 国产精品一区二区av麻豆| 久久精品无码一区二区三区| 国产h视频在线观看| 国精产品一区一区三区有限在线| 18禁日本黄无遮挡免费观看| 亚洲国产av无码一区二区三区| 一本无码av中文出轨人妻| 无码国产精品久久一区免费 | 超清av在线播放不卡无码| 国产午夜伦鲁鲁| 婷婷色婷婷开心五月四房播播久久 | 亚洲欧洲日本综合aⅴ在线| 久久久久亚洲精品天堂| 无码中文字幕人妻在线一区二区三区| 欧美天天综合色影久久精品| 日日麻批免费40分钟无码| 成人综合伊人五月婷久久| 自拍偷自拍亚洲精品播放| 国产精品久久久久乳精品爆| 久久久久国产精品免费免费搜索 | 国产三级精品三级| 国产乱码一二三区精品| 亚洲av成人无遮挡网站在线观看 | 人妻蜜と1~4中文字幕月野定规| 亚洲日韩欧美一区久久久久我| 一本无码人妻在中文字幕免费| 色吊丝中文字幕| 欧美内射深喉中文字幕| 精品人妻潮喷久久久又裸又黄 | 极品少妇第一次偷高潮哇哇大| 一区二区三区av波多野结衣| 无码av高潮喷水无码专区线| 肉岳疯狂69式激情的高潮| 国产97色在线 | 日韩| 成年女人毛片免费观看97| 色偷偷色噜噜狠狠网站30根|